This plexi is a complete replacement for the TE metal plate. It somes in 4mm and has rounded edges.




2 comments:

:oj said...

Hi Jochen, have you polished it manually? If yes: sounds like a mad job ;)

Arcadeforge said...

Yes, there is a polishing paste for acryl. The process is like this:

- Countersink the edges with a round bit
- Flame the edges to get a clear edge again
- Polish the edge with a acryl polish paste.